Brand Name : baililai
Model Number : CVD diamond wafer
Certification : 9001
Place of Origin : zhengzhou
MOQ : 10
Payment Terms : T/T
Packaging Details : Plastic box packaging
Hardness : 8000~10000Kg/mm2
Young’s modulus : 1.05GPa
Coefficient of thermal conductivity : 8~20W/(cm·K)
Tensile strength : 272 Kg/mm2
Compressive strength : 9.8×1013 Kg/mm2
Thermal expansion coefficient : 2.3×10-6/℃
Description :
The CVD diamond profile dresser blanks have good transparency,no cracking, good wear resistance,good impact resistance, the grinding wheel which grinded by CVD diamond profile dresser can make the workpiece highly polished, and can make sure the precise stable size.
Our regular sizes are 3.0mm*3.0mm ,3.5mm*3.0mm,4.0mm.*3.0mm ,Thickness has 1.0mm*2.0mm
Can also be cut into the shape desired by the customer according to the customer's requirements
![]() |